Specifications for the MIC SAS II 5800

Specification Description
Measurement range 0.5 - 75 μm
Porosity range 0.2 - 0.95
Compression accuracy < 0.05 mm
Environment
temperature
15 to 35 °C operating
0 to 50 °C non-operating
Repeatability ± 3%
Precision ± 3%
Power 30 W
Power supply

External power supply: 100 - 240 VAC ± 10%.
Power supplied to the instrument: 12 VDC @5A

Physical
Height 50 cm (19.5 in.)
Width 44 cm (17 in.)
Depth 27 cm (10.5 in.)
Weight 16 kg (34 lbs.)

In keeping with a policy of ongoing product improvement, specifications are subject to change without notice.

 