검색

Aero S

State-of-the-art dry powder dispersion

Setting new standards for dry powder dispersion, the Aero S has been designed from the ground up based upon fundamental powder dispersion theory. The modular design ensures rapid and reproducible dispersion of the widest range of samples from cohesive powders to fragile materials.

입자 크기 0.1 - 3500 µm †
Dispersion pressure range 0 - 4 bar
Pressure setting precision +/- 0.1 bar
Pressure setting accuracy +/- 0.03 bar
Feed rate range 0 - 58ms-2 (expressed as 0-100%)
Feed rate precision 2% FS
Materials in contact with the dispersant, additives and sample 316 stainless. 410 hardened stainless. Borosilicate glass. EPDM. PTFE. Polyurethane. Carbon filled acetal. Aluminum. Neoprene.
Maximum particle size 3500 µm †
Minimum time between measurements Less than 60 seconds †
Dimensions (W, D, H) 180mm x 260mm x 380mm
무게 10.5kg
전원 Supplied via the optical unit.
† Sample dependent

정보 요청