021-00000-00 |
Liquid Nitrogen Transfer System |
004-61004-00 |
Dewar |
350 mL, with safety sleeve and insulating cover |
230-31801-00 |
Dewar Cover |
Insulating, for standard Dewars |
230-31801-01 |
Dewar Cover |
Insulating, split, for cold trap Dewars |
004-25103-00 |
FERRULE |
Front, Teflon, for 1/4-in. (0.64-cm) OD tubing |
004-25104-00 |
FERRULE |
Rear, Nylon, for 1/4-in. (0.64-cm) OD tubing |
290-25842-00 |
Gas Extraction Assembly |
For calibration injections |
230-61002-00 |
Sample Tube |
Cylindrical bottom, 1 cm³ capacity |
230-61006-00 |
Sample Tube |
Cylindrical bottom, 1 cm³ capacity, package of 6 |
230-61007-00 |
Sample Tube |
Cylindrical bottom, 1 cm³ capacity, package of 12 |
230-61003-00 |
Sample Tube |
Capillary stem, 1 cm³ capacity |
230-61004-00 |
Sample Tube |
4.7 cm³ capacity |
230-61005-00 |
Sample Tube |
Monolith, up to 2 cm diameter x 3 cm long solid sample capacity |
230-61001-00 |
Sample Tube |
Micro U-tube, 0.1 cm³ capacity |
230-25821-00 |
Sample Tube Holder |
Complete with fittings and O-rings |
004-32004-00 |
Stopper |
For sample tube |
240-25853-00 |
Funnel |
|
230-32803-00 |
Weighing Support |
For supporting monolithic sample tubes |
230-32802-00 |
Weighing Support |
For supporting standard sample tubes |
004-25034-00 |
O-Ring |
Buna-N, Size 008, for sealing sample tube holder stems |
004-25466-00 |
O-Ring |
Buna-N, Size 010 for sealing sample tube holder and stems and cold trap stems |
231-26001-00 |
Heating Mantle with Thermocouple |
Glass Fiber, for FlowSorb III (350 ºC) |
230-26002-00 |
Heating Mantle with Thermocouple |
Glass Fiber, for monolith sample tubes (350 ºC) |
230-25808-00 |
Heating Mantle with Thermocouple |
Heating Mantle Clip |
230-26001-00 |
Heating Mantle with Thermocouple |
Glass Fiber, for standard sample tubes (350 ºC) |
004-61602-00 |
Calibration Syringe |
Precision, 1 mL |
004-61604-00 |
Calibration Syringe |
Precision, 10 mL |
004-61604-01 |
Calibration Syringe |
Replacement needles for 10 mL syringe |
004-61602-01 |
Calibration Syringe |
Replacement Injection Needles for 0.1 and 1 mL syringe |
004-32602-00 |
Septum |
For injection port |
231-42801-01 |
Manual |
Operator's, FlowSorb III |
231-33603-00 |
Extended Operation Supplies for the FlowSorb III. |
008-42001-00 |
Analytical Methods in Fine Particle Technology |
004-62230-58 |
CGA 580 fitting, 30 psig (Ar, He, Kr, N2) |
200-42901-00 |
Gas Adsorption Theory Poster |
200-42902-00 |
Gas Adsorption Apparatus Poster |