ISO 4652 RUBBER COMPOUNDING INGREDIENTS - CARBON BLACK - DETERMINATION OF Specific Surface Area |
https://www.iso.org/standard/75103.html |
FlowSorb III, Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Single-point Specific Surface Area |
ISO 8130-2 COATING POWDERS - PART 2: DETERMINATION OF DENSITY BY GAS COMPARISON PYKNOMETER (REFEREE METHOD) |
https://www.iso.org/standard/15201.html |
AccuPyc II
| Skeletal Density |
ISO 9277 DETERMINATION OF THE Specific Surface Area |
https://www.iso.org/standard/44941.html |
FlowSorb III, Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ISO 10070 METALLIC POWDERS - DETERMINATION OF ENVELOPE-Specific Surface Area |
https://www.iso.org/standard/74872.html |
SAS II |
Mean Particle Size and Envelope Specific Surface Area |
ISO 12154 DETERMINATION OF DENSITY BY VOLUMETRIC DISPLACEMENT - SKELETON DENSITY BY GAS PYCNOMETRY |
https://www.iso.org/standard/54731.html |
AccuPyc II
| Skeletal Density |
ISO 12800 NUCLEAR FUEL TECHNOLOGY - GUIDELINES ON THE MEASUREMENT OF THE SPECIFIC SURFACE AREA OF URANIUM OXIDE POWDERS BY THE BET METHOD |
https://www.iso.org/standard/66464.html |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ISO 13317-3 DETERMINATION OF PARTICLE SIZE DISTRIBUTION BY GRAVITATIONAL LIQUID SEDIMENTATION METHODS - PART 3: X-RAY GRAVITATIONAL TECHNIQUE |
https://www.iso.org/standard/30664.html |
SediGraph III Plus |
Particle Size Distribution |
ISO 13319 DETERMINATION OF PARTICLE SIZE DISTRIBUTIONS - ELECTRICAL SENSING ZONE METHOD |
https://www.iso.org/standard/42354.html |
Elzone II |
Particle Size Distribution |
ISO 13320 PARTICLE SIZE ANALYSIS - LASER DIFFRACTION METHODS |
https://www.iso.org/standard/69111.html |
Saturn DigiSizer II |
Particle Size Distribution |
ISO 15901-1 EVALUATION OF PORE SIZE DISTRIBUTION AND POROSITY OF SOLID MATERIALS BY MERCURY POROSIMETRY AND GAS ADSORPTION - PART 1: MERCURY POROSIMETRY |
https://www.iso.org/standard/56005.html |
AutoPore V |
Mercury Intrusion Porosimetry |
ISO 15901-2 PORE SIZE DISTRIBUTION AND POROSITY OF SOLID MATERIALS BY MERCURY POROSIMETRY AND GAS ADSORPTION - PART 2: ANALYSIS OF MESOPORES AND MACROPORES BY GAS ADSORPTION |
https://www.iso.org/standard/39386.html |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Pore Volume Distribution |
ISO 15901-3 PORE SIZE DISTRIBUTION AND POROSITY OF SOLID MATERIALS BY MERCURY POROSIMETRY AND GAS ADSORPTION - PART 3: ANALYSIS OF MICROPORES BY GAS ADSORPTION |
https://www.iso.org/standard/40364.html |
ASAP Series, TriStar II Plus, 3Flex |
Micropore Volume Distribution |
ISO 18753 FINE CERAMICS (ADVANCED CERAMICS, ADVANCED TECHNICAL CERAMICS) - DETERMINATION OF ABSOLUTE DENSITY OF CERAMIC POWDERS BY PYCNOMETER |
https://www.iso.org/standard/65414.html |
AccuPyc II
| Skeletal Density |
ISO 18757 FINE CERAMICS (ADVANCED CERAMICS, ADVANCED TECHNICAL CERAMICS) - DETERMINATION OF Specific Surface Area |
https://www.iso.org/standard/31903.html |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ISO 18852 RUBBER COMPOUNDING INGREDIENTS - DETERMINATION OF MULTIPOINT NITROGEN SURFACE AREA (NSA) AND STATISTICAL THICKNESS SURFACE AREA (STSA) |
https://www.iso.org/standard/66259.html |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ISO/AWI 24218-1 FINE BUBBLE TECHNOLOGY - CHARACTERIZATION OF FINE BUBBLES - PART 1: EVALUATION OF SIZE AND CONCENTRATION INDICES BY LASER DIFFRACTION METHOD |
https://www.iso.org/standard/78108.html |
Saturn DigiSizer II |
Particle Size Distribution |
ISO 24235 FINE CERAMICS (ADVANCED CERAMICS, ADVANCED TECHNICAL CERAMICS) - DETERMINATION OF PARTICLE SIZE DISTRIBUTION OF CERAMIC POWDERS BY LASER DIFFRACTION METHOD |
https://www.iso.org/standard/37114.html |
Saturn DigiSizer II |
Particle Size Distribution |
ASTM B330 Standard Test Methods for Estimating Average Particle Size of Metal Powders and Related Compounds Using Air Permeability |
https://www.astm.org/Standards/B330.htm |
SAS II |
Mean Particle Size and Envelope Specific Surface Area |
ASTM B761 Standard Test Method for Particle Size Distribution of Metal Powders and Related Compounds by X-Ray Monitoring of Gravity Sedimentation |
https://www.astm.org/Standards/B761.htm |
SediGraph III Plus |
Particle Size Distribution |
ASTM B822 Standard Test Method for Particle Size Distribution of Metal Powders and Related Compounds by Light Scattering |
https://www.astm.org/Standards/B822.htm |
Saturn DigiSizer II |
Particle Size Distribution |
ASTM B922 Standard Test Method for Metal Powder Specific Surface Area |
https://www.astm.org/Standards/B922.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM B923 Standard Test Method for Metal Powder Skeletal Density by Helium or Nitrogen Pycnometry |
https://www.astm.org/Standards/B923.htm |
AccuPyc II
| Skeletal Density |
ASTM C110 Standard Test Methods for Physical Testing of Quicklime, Hydrated Lime, and Limestone |
https://www.astm.org/Standards/C110.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex, AccuPyc II, SediGraph III Plus, Saturn II Plus |
Specific Surface Area |
ASTM C604 Standard Test Method for True Specific Gravity of Refractory Materials by Gas-Comparison Pycnometer |
https://www.astm.org/Standards/C604.htm |
AccuPyc II
| Skeletal Density |
ASTM C690 Standard Test Method for Particle Size Distribution of Alumina or Quartz Powders by Electrical Sensing Zone Technique |
https://www.astm.org/Standards/C690.htm |
Elzone II |
Particle Size Distribution |
ASTM C721 Standard Test Methods for Estimating Average Particle Size of Alumina and Silica Powders by Air Permeability |
https://www.astm.org/Standards/C721.htm |
SAS II |
Mean Particle Size and Envelope Specific Surface Area |
ASTM C958 Standard Test Method for Particle Size Distribution of Alumina or Quartz by X-Ray Monitoring of Gravity Sedimentation |
https://www.astm.org/Standards/C958.htm |
SediGraph III Plus |
Particle Size Distribution |
ASTM C1069 Standard Test Method for Specific Surface Area |
https://www.astm.org/Standards/C1069.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM C1070 Standard Test Method for Determining Particle Size Distribution of Alumina or Quartz by Laser Light Scattering |
https://www.astm.org/Standards/C1070.htm |
Saturn DigiSizer II |
Particle Size Distribution |
ASTM C1274 Standard Test Method for Advanced Ceramic Specific Surface Area |
https://www.astm.org/Standards/C1274.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM C1730 Standard Test Method for Particle Size Distribution of Advanced Ceramics by X-Ray Monitoring of Gravity Sedimentation |
https://www.astm.org/Standards/C1730.htm |
SediGraph III Plus |
Particle Size Distribution |
ASTM D70 Standard Test Method for Density of Semi-Solid Asphalt Binder (Pycnometer Method) |
https://www.astm.org/Standards/D70.htm |
AccuPyc II
| Skeletal Density |
ASTM D1993 Standard Test Method for Precipitated Silica-Surface Area by Multipoint BET Nitrogen Adsorption |
https://www.astm.org/Standards/D1993.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM D2638 Standard Test Method for Real Density of Calcined Petroleum Coke by Helium Pycnometer |
https://www.astm.org/Standards/D2638.htm |
AccuPyc II
| Skeletal Density |
ASTM D3663 Standard Test Method for Surface Area of Catalysts and Catalyst Carriers |
https://www.astm.org/Standards/D3663.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM D3907/D3907M Standard Test Method for Testing Fluid Catalytic Cracking (FCC) Catalysts by Microactivity Test |
https://www.astm.org/Standards/D3907.htm |
Flow Reactor (FR) Series and Multi Reactor (MR) Series |
Fluid Cracking Catalyst Activiry |
ASTM D3908 Standard Test Method for Hydrogen Chemisorption on Supported Platinum Catalysts by Volumetric Vacuum Method |
https://www.astm.org/Standards/D3908.htm |
ASAP 2020 Plus Chemi, 3Flex Chemi, 3 Flex TCD, ChemiSorb HTP |
Chemisorption Catalyst Surface Area and Percent Dispersion |
ASTM D4222 Standard Test Method for Determination of Nitrogen Adsorption and Desorption Isotherms of Catalysts and Catalyst Carriers by Static Volumetric Measurements |
https://www.astm.org/Standards/D4222.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Physisorption Isotherms |
ASTM D4284 Standard Test Method for Determining Pore Volume Distribution of Catalysts and Catalyst Carriers by Mercury Intrusion Porosimetry |
https://www.astm.org/Standards/D4284.htm |
AutoPore V |
Mercury Intrusion Porosimetry |
ASTM D4365 Standard Test Method for Determining Micropore Volume and Zeolite Area of a Catalyst |
https://www.astm.org/Standards/D4365.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM D4404 Standard Test Method for Determination of Pore Volume and Pore Volume Distribution of Soil and Rock by Mercury Intrusion Porosimetry |
https://www.astm.org/Standards/D4404.htm |
AutoPore V |
Mercury Intrusion Porosimetry |
ASTM D4438 Standard Test Method for Particle Size Distribution of Catalysts and Catalyst Carriers by Electronic Counting |
https://www.astm.org/Standards/D4438.htm |
Elzone II |
Particle Size Distribution |
ASTM D4464 Standard Test Method for Particle Size Distribution of Catalytic Materials by Laser Light Scattering |
https://www.astm.org/Standards/D4464.htm |
Saturn DigiSizer II |
Particle Size Distribution |
ASTM D4567 Standard Test Method for Single-Point Determination of Specific Surface Area |
https://www.astm.org/Standards/D4567.htm |
FlowSorb III |
Single-point Specific Surface Area |
ASTM D4641 Standard Practice for Calculation of Pore Size Distributions of Catalysts and Catalyst Carriers from Nitrogen Desorption Isotherms |
https://www.astm.org/Standards/D4641.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Pore Volume Distribution |
ASTM D4780 Standard Test Method for Determination of Low Surface Area of Catalysts and Catalyst Carriers by Multipoint Krypton Adsorption |
https://www.astm.org/Standards/D4780.htm |
ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM D4824 Standard Test Method for Determination of Catalyst Acidity by Ammonia Chemisorption |
https://www.astm.org/Standards/D4824.htm |
ASAP 2020 Plus Chemi, 3Flex Chemi, 3 Flex TCD, ChemiSorb HTP |
Chemisorption Catalyst Surface Area and Percent Dispersion |
ASTM D4892 Standard Test Method for Density of Solid Pitch (Helium Pycnometer Method) |
https://www.astm.org/Standards/D4892.htm |
AccuPyc II
| Skeletal Density |
ASTM D5154/D5154M Standard Test Method for Determining Activity and Selectivity of Fluid Catalytic Cracking (FCC) Catalysts by Microactivity Test |
https://www.astm.org/Standards/D5154.htm |
Flow Reactor (FR) Series and Multi Reactor (MR) Series |
Fluid Cracking Catalyst Activiry |
ASTM D5550 Standard Test Method for Specific Gravity of Soil Solids by Gas Pycnometer |
https://www.astm.org/Standards/D5550.htm |
AccuPyc II
| Skeletal Density |
ASTM D5604 Standard Test Methods for Precipitated Silica-Surface Area by Single Point B.E.T. Nitrogen Adsorption |
https://www.astm.org/Standards/D5604.htm |
FlowSorb III, Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Single-point Specific Surface Area |
ASTM D5861 Standard Guide for Significance of Particle Size Measurements of Coating Powders |
https://www.astm.org/Standards/D5861.htm |
Saturn DigiSizer II |
Particle Size Distribution |
ASTM D5965 Standard Test Methods for Density of Coating Powders |
https://www.astm.org/Standards/D5965.htm |
AccuPyc II
| Skeletal Density |
ASTM D6093 Standard Test Method for Percent Volume Nonvolatile Matter in Clear or Pigmented Coatings Using a Helium Gas Pycnometer |
https://www.astm.org/Standards/D6093.htm |
AccuPyc II
| Skeletal Density |
ASTM D6226 Standard Test Method for Open Cell Content of Rigid Cellular Plastics |
https://www.astm.org/Standards/D6226.htm |
AccuPyc II
| Open and Closed Cell Content of Foam |
ASTM D6556 Standard Test Method for Carbon Black-Total and External Surface Area by Nitrogen Adsorption |
https://www.astm.org/Standards/D6556.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM D6761 Standard Test Method for Determination of the Total Pore Volume of Catalysts and Catalyst Carriers |
https://www.astm.org/Standards/D6761.htm |
AutoPore V and AccuPyc II
| Total Pore Volume |
ASTM D7854 Standard Test Method for Carbon Black-Void Volume at Mean Pressure |
https://www.astm.org/Standards/D7854.htm |
DVVA II |
Dynamic Void Volume |
ASTM D7891-15 Standard Test Method for Shear Testing of Powders Using the Freeman Technology FT4 |
https://www.astm.org/Standards/D7891.htm |
FT4 |
Powder Shear Characterization |
ASTM D8097 Standard Test Method for Determination of Bulk Density for Specific Size Fractions of Calcined Petroleum Coke Using a Transaxial Pressure Pycnometer |
https://www.astm.org/Standards/D8097.htm |
GeoPyc II |
Transverse Axial Pressure (T.A.P.) Density |
ASTM D8325 Standard Guide for Evaluation of Nuclear Graphite Surface Area and Porosity by Gas Adsorption Measurements |
https://www.astm.org/Standards/D8325.htm |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM E2864 Standard Test Method for Measurement of Airborne Metal Oxide Nanoparticle Surface Area Concentration in Inhalation Exposure Chambers using Krypton Gas Adsorption |
https://www.astm.org/Standards/E2864.htm |
ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |
ASTM E2980 Standard Test Methods for Estimating Average Particle Size of Powders Using Air Permeability |
https://www.astm.org/Standards/E2980.htm |
SAS II |
Mean Particle Size and Envelope Specific Surface Area |
ASTM F2149 Standard Test Method for Automated Analyses of Cells-the Electrical Sensing Zone Method of Enumerating and Sizing Single Cell Suspensions |
https://www.astm.org/Standards/F2149.htm |
Elzone II |
Particle Size Distribution |
WK61828 Carbon Monoxide on Supported Platinum on Alumina Catalysts using Manometric Method |
https://www.astm.org/DATABASE.CART/WORKITEMS/WK61828.htm |
ASAP 2020 Plus Chemi, 3Flex Chemi, 3 Flex TCD, ChemiSorb HTP |
Chemisorption Catalyst Surface Area and Percent Dispersion |
WK17123 New Test Method for Test Method for Carbon Monoxide Chemisorption on Supported Platinum on Alumina Catalysts using Dynamic Flow Method |
https://www.astm.org/DATABASE.CART/WORKITEMS/WK17123.htm |
AutoChem II |
Chemisorption Catalyst Surface Area and Percent Dispersion |
WK71859 Carbon Monoxide Chemisorption on Supported Platinum on Alumina Catalysts using Static Vacuum Method |
https://www.astm.org/DATABASE.CART/WORKITEMS/WK71859.htm |
ASAP 2020 Plus Chemi, 3Flex Chemi, 3 Flex TCD, ChemiSorb HTP |
Chemisorption Catalyst Surface Area and Percent Dispersion |
WK71860 Acid Site Characterization on Zeolites Using Dynamic Flow Method |
https://www.astm.org/DATABASE.CART/WORKITEMS/WK71860.htm |
AutoChem II |
Acid Site Characterization |
WK69721 Measuring the Permeability of Powders as a Function of Consolidation Using the Freeman Technology FT4 |
https://www.astm.org/DATABASE.CART/WORKITEMS/WK69721.htm |
FT4 |
Powder Permeability |
WK69886 The Dynamic Testing of Powders using the Freeman Technology FT4 |
https://www.astm.org/DATABASE.CART/WORKITEMS/WK69886.htm |
FT4 |
Powder Rheology |
USP <267> Porosimetry by Mercury Intrusion |
https://www.usp.org/harmonization-standards/pdg/general-chapters/porosimetry-mercury-intrusion |
AutoPore V |
Mercury Intrusion Porosimetry |
USP <429> Laser Diffraction Measurement of Particle Size |
https://www.usp.org/harmonization-standards/pdg/general-chapters/laser-diffraction-measurement-particle-size |
Saturn DigiSizer II |
Particle Size Distribution |
USP <699> Gas Pycnometric Density of Solids |
https://www.usp.org/harmonization-standards/pdg/general-chapters/gas-pycnometric-density-solids |
AccuPyc II
| Skeletal Density |
USP <846> Specific Surface Area |
https://www.usp.org/harmonization-standards/pdg/general-chapters/specific-surface-area |
Gemini VII, ASAP Series, TriStar II Plus, 3Flex |
Specific Surface Area |