Quantifying the impact of temperature on bulk powder properties such as flowability for more effective process optimization.
In this webinar, Laura Shaw, Applications Specialist at Freeman Technology, will discuss how temperature affects powder behavior and consider the requirements for testing at elevated temperature. Experimental data will be presented demonstrating the effect of temperature changes on the flowability of a pharmaceutical excipient and an AM feedstock, and highlighting the challenges of predicting any impact.