Suche

Aero M

Routine particle size analysis for bulk dry powder samples

The Aero M dry powder disperser enables bulk dry powder samples to be measured using the Mastersizer laser diffraction particle size analyzer. Its simple design ensures that it is easy to use and maintain, delivering robust, reproducible particle size distribution measurements as part of routine production or quality control operations.

Partikelgröße 0.1 - 1000 µm †
Dispersion pressure range 0 - 4 bar
Pressure setting precision +/- 0.1 bar
Pressure setting accuracy +/- 0.03 bar
Feed rate range 0 - 58ms-2 (expressed as 0-100%)
Feed rate precision 2% FS
Materials in contact with sample 316 stainless. 410 hardened stainless. Borosilicate glass. EPDM. PTFE. Polyurethane. Carbon filled acetal. Aluminum. Neoprene.
Maximum particle size 1000 µm †
Minimum time between measurements Less than 60 seconds †
Dimensions (W, D, H) 180mm x 260mm x 380mm
Gewicht 10.5kg
Strom Supplied via the optical unit.
† Sample dependent. Relates to the use of the unit with the Mastersizer 3000E, which also has a upper size limit of 1000 µm.