The Aero funnel sample feeder is designed to help users achieve rapid, reproducible bulk dry powder particle size measurements by allowing samples to be added directly to the Aero S and Aero M dry powder dispersion units without opening the dispersion unit lid. This speeds up and simplifies the process of introducing samples for analysis, decreasing the time required to obtain results.
| Size range | 0.1 - 3500µm*† |
|---|---|
| Maximum sample mass measured | 15g* |
| Dispersion pressure range | 0 - 4 bar |
| Pressure setting precision | +/- 0.1 bar |
| Pressure setting accuracy | +/- 0.03 bar |
| Feed rate range | 0 - 58ms-2 (expressed as 0-100%) |
| Feed rate precision | 2% FS |
| Materials in contact with sample | 316 stainless
|
| Maximum particle size | 3500 µm† |
| Minimum time between measurements | less than 60 sec * |
| Dimensions (W, D, H) | 180mm x 260mm x 380mm |
| 重量 | 10.5kg |
| Power Supply | Supplied via the Mastersizer optical unit |
| 備考 | * Sample dependent.
† Relates to the use of the unit with the Mastersizer 3000. Upper particle size limit is 1000µm when used with the Aero M on the Mastersizer 3000E. Note: Magnetic materials cannot be measured using the funnel sample feeder as the feeder includes magnetic components |