AccuPore

The
easiest
most accurate
most versatile
measurement of through-porosity

Overview

Capillary Flow Porometry
Through-pore Size Distribution​

Capillary Flow Porometry (CFP) — also known as Gas Liquid Porometry (GLP) — is a fast, reliable method to determine the size and relative abundance of throughpores in sheets and membranes. This pressure-based technique measures the minimum diameter of a pore, averaging over a significant test area, without the need for model-fitting or image processing. Measurements are fast, sample preparation takes less than 30 seconds, and no mercury is involved.

SAMPLE PREPARATION
Sample is wetted with a special fluid that fills every pore.
WET CURVE
Gas pressure is applied to force the wetting fluid from the pores. Larger pores open at lower pressure.
Increasing pressure opens more, smaller pores, increasing gas flow rate through the sample.
DRY CURVE
After all pores are opened and all of the wetting fluid has been expelled from the sample, flow across the
un-wetted dry film is measured.

Key Measurements

Bubble Point, Largest Pore:​

The lowest pressure at which flow occurs.

Mean Flow Pore:

Intersection of the wet curve with the dry curve divided by two — the half-dry curve.

Smallest Pore:

Intersection of the wet curve with the dry curve.

Pore Size Distribution:

A continuous distribution of the differential and cumulative pore size reveals the overall structure of pores in a membrane.

Features

The SmartFlow system provides precision control for porosimetry in either pressure ramp or step modes. The option to perform measurements in either mode ensures the correct measurement is available from routine qualification to detailed characterization.

Pressure Ramp

Increasing pressure at a steady rate shortens measurement time, provides a highly repeatable measurement, and produces data points tightly spaced in pressure.


Routine operation, producing high resolution, highly repeatable data, in a short time.

Pressure Step

Pausing at each pressure for equilibration allows all pores of a given diameter to fully empty before moving to the next pressure, regardless of pore length or tortuosity.


Highest possible resolution and absolute pore size accuracy especially for complex pores and thick sheets.

High resolution, low noise pressure-flow curves enable highly detailed pore size distributions that reflect physical pore architecture WITHOUT curve fitting or post-processing.

The AccuPore features SmartFlow, an advanced flow control system that guarantees the most precise pressure control, highest sensitivity, and lowest signal noise. High-resolution 24-bit electronics operated at 20 Hz for optimal signal quality and system response. With eight complementary transducers and controllers, SmartFlow delivers the most responsive and stable performance, even during rapidly changing conditions such as pore opening.

1

Flexible easy-to-use
sample chamber

2

Intuitive Breeze Interface

3

Convenient USB

4

High-speed control, collection, and data processing

5

MIC Net

6

Auto-switching gas supply

1. Flexible easy-to-use sample chamber

for simple sample loading including samples from 13 mm to 47 mm diameter.

2. Intuitive Breeze Interface

makes it easy to measure samples and review results with or without a PC.

3. Convenient USB

access for data transfer or peripheral device integration. Even more ports at the back of the instrument.

4. High-speed control, collection, and data processing

provides the most accurate pressure control, highest curve resolution, and most detailed pore size distribution by processing measurements at up to 20 Hz.

5. MIC Net

empowers your lab to operate as one by synchronizing results and methods across AccuPore instruments. Laboratory network connection provides simple data retrieval and LIMS integration.

6.Auto-switching gas supply

reduces cost of operation by using low pressure compressed air when suitable, allowing high pressure bottled gas tanks to last longer.

Why AccuPore?

The Most Accurate Bubble Point

SmartFlow also enables direct measurement of true bubble point through a proprietary flow-controlled method that provides unmatched accuracy and repeatability. Conventional estimates of bubble point from pressure ramps lack sensitivity and can underestimate the largest pore diameter. SmartFlow ensures precise bubble point measurements, typically much better than ±1%.

First Bubble Point Size (µm)
Measurement Track-etched
membrane A
Track-etched
membrane B
Track-etched
membrane C
Track-etched
membrane D
1 1.153 0.309 0.092 0.055
2 1.151 0.309 0.092 0.055
3 1.170 0.308 0.092 0.054
4 1.164 0.309 0.091 0.054
5 1.162 0.308 0.092 0.054
6 1.180 0.309 0.091 0.054
7 1.166 0.309 0.091 0.054
8 1.178 0.310 0.091 0.054
9 1.175 0.308 0.090 0.054
10 1.165 0.309 0.090 0.054
Average 1.166 0.309 0.091 0.054
Relative standard deviation 0.83% 0.22% 0.72% 0.54%

Run, Review, Report – At Your Fingertips

The intuitive Breeze touch interface gives you everything you need at your fingertips. Perform a measurement, review past results, send a report to print or to LIMS (PDF, text, or Excel) with the touch of a finger. Save space in your lab by eliminating a PC from the bench.

Prefer to work from a PC nearby or in your office? You can do that too! Execute measurements, view status of multiple instruments, or review results…anywhere.

  • Automatic results generation and retrieval:
    • Largest pore diameter (bubble point)
    • Mean pore diameter
    • Smallest pore diameter
    • Pore size distribution
  • Tabular review of detailed test data
  • Porometry and Pore Flow Distribution curve display
  • Generate reports including print and export to file
  • Export to file via network or USB

Measure Right, Without Questions

Different materials require specific operating conditions. Whether measuring bubble point, routine pore size distribution, or detailed structure analysis, the AccuPore simplifies it all. With SmartFlow pressure control, it doesn’t take an expert to operate. Fewer settings and adjustable parameters make method development fast and worry-free. Use the Method Library to define, store, and recall your methods easily, so you always measure the same way — the right way.

Cut Costs With Smart Gas Selection

Reduce operational costs with intelligent gas source selection. The AccuPore uses a compressor for low-pressure operations (bubble point measurement and large pores) and switches to high-pressure bottled gas for analysis of small pores. This reduces the need for expensive highpressure gas, lowering your recurring costs.

Move Quickly From Data to Decision With MicroActive Analysis and Reporting

MicroActive software streamlines data processing, offering detailed plotting, analysis and reporting, including statistical process control charts and results overlays. Gas-liquid CFP is a direct complement to mercury intrusion porosimetry (MIP), providing a rich description of pore architecture. Only with MicroActive can you easily co-plot results from the AccuPore CFP and AutoPore MIP to fully describe the pore characteristics of a material.

>
<

Applications

Battery and Fuel Cell Separators and Membranes

Optimize the rate of ion transport and physical separation to ensure device...

+

Filtration

Predict and ensure size-based selectivity and mass-transfer rate by optimizing the number...

+
Non-Wovens

Non-Wovens

Often characterized by a broad distribution of pore sizes due to their...

+

Metal and Ceramics

Preferred for thermal, physical, and chemical resistance, these materials often have highly...

+

Capabilities

Technique

Capillary Flow Porometry
ASTM F316

Measurement Method

Pressure Ramp
Pressure Step

Pore Size Range

0.013 µm to 500 µm*

Max Pressure

500 psi / 35 bar

Max Flow Rate

200 L/min

Analysis Gas Supply

Air or N2

Operational Modes

Bubble Point (Direct Measure)
Capillary Flow Porometry by:
Dry/Wet, Wet/Dry, Wet/Calculated Dry

Physical Dimensions

57 cm Wide x 61 cm Deep

Curve Resolution

>1000 data points per run
20 Hz internal data processing speed

Sample Sizes

25 mm diameter standard
Adapters available for 13 mm, 47 mm diameter

Provided specifications were valid as taken from available documents at time of publication. These specifications may change without notice and are only provided as a general reference

Highlights

  • Automatic gas source selection reduces cost of operation
  • Built-in Breeze touchscreen UI with full standalone instrument control and data analysis
  • Remote PC control and data analysis over network connection
  • MicroActive software: Advanced analysis and reporting, coplot with complementary porosity data
  • Data transfer via USB and wired (ethernet) or wireless (Wi-Fi) network communication
  • Network printing including wireless via Airprint for simple report creation

Request Info

Request a quote or talk to an expert for more information