Search
Method: 
  • Powder Flow

Understanding The Flowability Of Spray Dried Milk Powders Using The FT4 Powder Rheometer®

Introduction

Milk powders produced by spray drying are used across the food industry to make products
ranging from confectionery and baked goods to soups, sauces, and beverages; they are also
supplied directly to consumers. The flow properties of these powders define their utility and
by extension their value, notably for efficient and effective food processing. Powders that flow
easily and reliably through the production chain maximise industrial throughput, eliminating the
unplanned stoppages and inefficiencies that can degrade profitability. Understanding how to
make milk powders with superior flow properties is therefore advantageous, with lipid content
known to be highly influential though other factors such as moisture content and particle size also
have a role to play in defining flow behaviour.

In this study by researchers at the Universite de Lorraine, Nancy, France, the flowability of spraydried milk powders was investigated as a function of feed concentrate composition and an
aeration pre-treatment [1]. Spray-dried powders of varying lipid content — 1.5%, 14% and 26% —
were produced from skimmed, semi-skimmed and whole milk concentrates respectively, prepared
by reconstituting skimmed and whole milk powders. These three samples were compared with
aerated analogues, produced by whipping samples of each of the concentrates prior to spraydrying under strictly comparable conditions. Dynamic and shear flow properties were measured
for all six spray-dried milk powders using the FT4 Powder Rheometer®. The results show valuable
correlation between feed concentrate properties and process-relevant flow properties.

Flowability

Basic Flowability Energy (BFE) values quantify a powder’s propensity to flow under confined or
forcing conditions, when in a low to moderately stressed state. BFE values have been securely
associated with, for example, blending performance and flow through the feedframe of a dosing
system or tableting press making them relevant to food processing operations. Furthermore, they
are highly differentiating, often able to detect even small differences in samples that other flow
properties classify as identical or highly similar.

For these milk powders, BFE was found to increase with lipid content (skimmed 1.5%, semiskimmed: 14%, whole: 26%) for untreated, and also for the samples prepared from treated/aerated
concentrates. With these data, we can see that aeration has a strong influence on BFE, increasing
resistance to flow.

Basic Flowability Energy
High Stress Cohesion

Shear properties such as cohesion quantify the behaviour of consolidated powders under relatively high stress and are pertinent to hopper discharge performance. These results provide a different perspective on the samples indicating minimal differentiation between the semiskimmed and whole milk powders but notably less cohesion in the skimmed sample. For all three samples aeration has only a marginal effect on sample behaviour.

Physicochemical properties measured for the milk powders provide insight into these observed trends. For example, semi-skimmed and whole milk powders were observed to have high and over-representative surface lipid content. Increased surface ‘stickiness’ as a result of lipid distribution therefore provides a rationale for the high cohesion and resistance to flow observed with the semi-skimmed and whole milk powders, relative to skimmed. The more marked effect observed under high stress conditions may be the result of free fat release at the powder surface under consolidating load.

Aeration results in more uniform lipid dispersion, but at the same time gives rise to narrower particle size distributions centred on a finer particle size. This latter trend potentially impacts particle packing, an important behaviour with respect to BFE values and may therefore help to explain the trends in flow behaviour observed under low stress conditions; high consolidation potentially masks the differences induced by pretreatment.

Crucially, however, the observed trends provide insight into how different milk powders will behave in process. Low lipid content is clearly conducive to low cohesion and good flowability in hoppers and silos, and indeed more generally while processors looking to aerate dairy concentrates to improve characteristics such as wettability and solubility should be wary of the possibility of simultaneously compromising flowability and, by extension processibility.

Conclusion

The results presented here illustrate the value of measuring dynamic and shear powder
properties to gather process-relevant insight into different milk powders and the impact of
concentrate pretreatment. This type of multivariate analysis provides a level of detail unobtainable
via simple, single parameter powder testing methods and can be highly effective in supporting
the development of optimal ingredients for food processing.

References

[1] T. Fournaise, J. Burgain, C. Perroud, J. Scher, G. Gaiani, J. Petit ‘Impact of formulation on reconstitution and flowability of spray-dried milk powders’ Powder Technology 372 (2020) 107-116.