Specification
X-ray generation
X-ray generator | 4 kW (max 60 kV, max 100 mA) |
---|---|
Line/point focus switch | Easy and quick, without tooling |
Goniometer
Range | Maximum usable range (depending on accessories): -111 |
---|---|
Smallest addressable increment | 0.0001° |
Reproducibility | < 0.0002° |
2θ linearity | Equal or better than ± 0.01° |
Maximum speed | 15 deg/s |
Resolution | 0.026° FWHM on LaB₆ |
Sample stages
Ambient sample stages |
|
---|---|
Non-ambient sample stages |
|
Detectors
Point detectors | Proportional counter (20 x 24 mm)
Scintillation detector (30 mm Ø) |
---|---|
Strip detectors | PIXcel1D, 256 strips of 55 μm ‘all live’, compatible with Cr to Cu radiation |
Area detectors | PIXcel3D, 256 x 256 pixels of 55 μm, compatible with Cr to Cu radiation
GaliPIX3D, 501 x 465 pixels of 60 μm, compatible with Co to Ag radiation (with 100% efficiency) |
Cabinet
Dimensions | 1400 (w) × 1162 (d) × 1947 (h) mm.
The instrument is on wheels. It can pass a 989 mm door opening. For transportation the minimum achievable instrument width is 867 mm. |
---|---|
Weight | 1150 kg |
Internal dimensions | 1360 (w) × 1100 (h) mm, allowing access to the experimental area by at least four people simultaneously (ideal for teaching) |
Radiation levels | Radiation level less than 1 microSievert per hour, measured at 10 cm distance, determined with a Mo source @ 60 kV, 50 mA. No power restrictions with all anode types |
External cooling water supply | 4 - 6 liters/min, pressure up to 8 bar, temperature 15 to 35 °C > dew point |
Compressed air supply | House line, compressor or air bottle; 2-5 bar (0.2 - 0.5 MPa) |
Power Supply | Single phase 210 – 230 V (with ± 10% grid variations); 50/60 Hz |
Power consumption | Max. 4.6 kVA without controllers for optional equipment |