Buscar en

Industry standards

Find your required industry standards organization and reference number then select the applicable Malvern Panalytical products.

Micromeritics Products by Industry Standards

Estándar Method Relevant Instrument(s) Método de caracterización
ISO 4652 RUBBER COMPOUNDING INGREDIENTS - CARBON BLACK - DETERMINATION OF Specific Surface Area 3Flex, AccuPore, ASAP 2460 & 2425, TriStar II Plus Single-point Specific Surface Area
ISO 8130-2 COATING POWDERS - PART 2: DETERMINATION OF DENSITY BY GAS COMPARISON PYKNOMETER (REFEREE METHOD) AccuPyc Densidad esquelética
ISO 9277 DETERMINATION OF THE Specific Surface Area Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ISO 10070 METALLIC POWDERS - DETERMINATION OF ENVELOPE-Specific Surface Area SAS Mean Particle Size & Envelope Surface Area
ISO 12154 DETERMINATION OF DENSITY BY VOLUMETRIC DISPLACEMENT - SKELETON DENSITY BY GAS PYCNOMETRY AccuPyc Densidad esquelética
ISO 12800 NUCLEAR FUEL TECHNOLOGY - GUIDELINES ON THE MEASUREMENT OF THE SPECIFIC SURFACE AREA OF URANIUM OXIDE POWDERS BY THE BET METHOD SediGraph Distribución del tamaño de las partículas
ISO 13319 DETERMINATION OF PARTICLE SIZE DISTRIBUTIONS - ELECTRICAL SENSING ZONE METHOD Elzone II 5390 Distribución del tamaño de las partículas
ISO 13320 PARTICLE SIZE ANALYSIS - LASER DIFFRACTION METHODS Saturn DigiSizer II 5205 Distribución del tamaño de las partículas
ISO 15901-1 EVALUATION OF PORE SIZE DISTRIBUTION AND POROSITY OF SOLID MATERIALS BY MERCURY POROSIMETRY AND GAS ADSORPTION - PART 1: MERCURY POROSIMETRY AutoPore V Porosimetría de intrusión de mercurio
ISO 15901-2 PORE SIZE DISTRIBUTION AND POROSITY OF SOLID MATERIALS BY MERCURY POROSIMETRY AND GAS ADSORPTION - PART 2: ANALYSIS OF MESOPORES AND MACROPORES BY GAS ADSORPTION Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Distribución del volumen de poros
ISO 15901-3 PORE SIZE DISTRIBUTION AND POROSITY OF SOLID MATERIALS BY MERCURY POROSIMETRY AND GAS ADSORPTION - PART 3: ANALYSIS OF MICROPORES BY GAS ADSORPTION ASAP 2460 & 2425, TriStar II Plus, 3Flex Distribución del volumen de microporos
ISO 18753 FINE CERAMICS (ADVANCED CERAMICS, ADVANCED TECHNICAL CERAMICS) - DETERMINATION OF ABSOLUTE DENSITY OF CERAMIC POWDERS BY PYCNOMETER AccuPyc, AccuPyc II 1345 Densidad esquelética
ISO 18757 FINE CERAMICS (ADVANCED CERAMICS, ADVANCED TECHNICAL CERAMICS) - DETERMINATION OF Specific Surface Area Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ISO 18852 RUBBER COMPOUNDING INGREDIENTS - DETERMINATION OF MULTIPOINT NITROGEN SURFACE AREA (NSA) AND STATISTICAL THICKNESS SURFACE AREA (STSA) Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ISO/AWI 24218-1 FINE BUBBLE TECHNOLOGY - CHARACTERIZATION OF FINE BUBBLES - PART 1: EVALUATION OF SIZE AND CONCENTRATION INDICES BY LASER DIFFRACTION METHOD Saturn DigiSizer II 5205 Distribución del tamaño de las partículas
ISO 24235 FINE CERAMICS (ADVANCED CERAMICS, ADVANCED TECHNICAL CERAMICS) - DETERMINATION OF PARTICLE SIZE DISTRIBUTION OF CERAMIC POWDERS BY LASER DIFFRACTION METHOD Saturn DigiSizer II 5205 Distribución del tamaño de las partículas
ASTM B330 Standard Test Methods for Estimating Average Particle Size of Metal Powders and Related Compounds Using Air Permeability SAS Mean Particle Size & Envelope Specific Surface Area
ASTM B761 Standard Test Method for Particle Size Distribution of Metal Powders and Related Compounds by X-Ray Monitoring of Gravity Sedimentation SediGraph Distribución del tamaño de las partículas
ASTM B922 Standard Test Method for Metal Powder Specific Surface Area Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM B923 Standard Test Method for Metal Powder Skeletal Density by Helium or Nitrogen Pycnometry AccuPyc, AccuPyc II 1345 Densidad esquelética
ASTM C110 Standard Test Methods for Physical Testing of Quicklime, Hydrated Lime, and Limestone Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex, AccuPyc, AccuPyc II 1345, SediGraph, Saturn DigiSizer II 5205 Superficie específica
ASTM C604 Standard Test Method for True Specific Gravity of Refractory Materials by Gas-Comparison Pycnometer AccuPyc, AccuPyc II 1345 Densidad esquelética
ASTM C690 Standard Test Method for Particle Size Distribution of Alumina or Quartz Powders by Electrical Sensing Zone Technique Elzone II 5390 Distribución del tamaño de las partículas
ASTM C721 Standard Test Methods for Estimating Average Particle Size of Alumina and Silica Powders by Air Permeability SAS Mean Particle Size & Envelope Specific Surface Area
ASTM C958 Standard Test Method for Particle Size Distribution of Alumina or Quartz by X-Ray Monitoring of Gravity Sedimentation SediGraph Distribución del tamaño de las partículas
ASTM C1069 Standard Test Method for Specific Surface Area Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM C1070 Standard Test Method for Determining Particle Size Distribution of Alumina or Quartz by Laser Light Scattering Saturn DigiSizer II 5205 Distribución del tamaño de las partículas
ASTM C1274 Standard Test Method for Advanced Ceramic Specific Surface Area Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM C1730 Standard Test Method for Particle Size Distribution of Advanced Ceramics by X-Ray Monitoring of Gravity Sedimentation SediGraph Distribución del tamaño de las partículas
ASTM D70 Standard Test Method for Density of Semi-Solid Asphalt Binder (Pycnometer Method) AccuPyc, AccuPyc II 1345 Densidad esquelética
ASTM D1993 Standard Test Method for Precipitated Silica-Surface Area by Multipoint BET Nitrogen Adsorption Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM D2638 Standard Test Method for Real Density of Calcined Petroleum Coke by Helium Pycnometer AccuPyc, AccuPyc II 1345 Densidad esquelética
ASTM D3663 Standard Test Method for Surface Area of Catalysts and Catalyst Carriers Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM D3907/D3907M Standard Test Method for Testing Fluid Catalytic Cracking (FCC) Catalysts by Microactivity Test Flow Reactor (FR) Fluid Cracking Catalyst Activity
ASTM D3908 Standard Test Method for Hydrogen Chemisorption on Supported Platinum Catalysts by Volumetric Vacuum Method ASAP 2020 Plus, ASAP 2020, 3Flex, ChemiSorb HTP Chemisorption; Catalyst Surface Area and Percent Dispersion
ASTM D4222 Standard Test Method for Determination of Nitrogen Adsorption and Desorption Isotherms of Catalysts and Catalyst Carriers by Static Volumetric Measurements Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Isotermas de fisisorción
ASTM D4284 Standard Test Method for Determining Pore Volume Distribution of Catalysts and Catalyst Carriers by Mercury Intrusion Porosimetry AutoPore V Porosimetría de intrusión de mercurio
ASTM D4365 Standard Test Method for Determining Micropore Volume and Zeolite Area of a Catalyst Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM D4404 Standard Test Method for Determination of Pore Volume and Pore Volume Distribution of Soil and Rock by Mercury Intrusion Porosimetry AutoPore V Porosimetría de intrusión de mercurio
ASTM D4438 Standard Test Method for Particle Size Distribution of Catalysts and Catalyst Carriers by Electronic Counting Elzone II 5390 Distribución del tamaño de las partículas
ASTM D4464 Standard Test Method for Particle Size Distribution of Catalytic Materials by Laser Light Scattering Saturn DigiSizer II 5205 Distribución del tamaño de las partículas
ASTM D4641 Standard Practice for Calculation of Pore Size Distributions of Catalysts and Catalyst Carriers from Nitrogen Desorption Isotherms Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Distribución del volumen de poros
ASTM D4780 Standard Test Method for Determination of Low Surface Area of Catalysts and Catalyst Carriers by Multipoint Krypton Adsorption ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM D4824 Standard Test Method for Determination of Catalyst Acidity by Ammonia Chemisorption ASAP 2020 Plus, 3Flex, ChemiSorb HTP Chemisorption; Catalyst Surface Area and Percent Dispersion
ASTM D4892 Standard Test Method for Density of Solid Pitch (Helium Pycnometer Method) AccuPyc II 1345 Densidad esquelética
ASTM D5154/D5154M Standard Test Method for Determining Activity and Selectivity of Fluid Catalytic Cracking (FCC) Catalysts by Microactivity Test Flow Reactor (FR) Fluid Cracking Catalyst Activity
ASTM D5550 Standard Test Method for Specific Gravity of Soil Solids by Gas Pycnometer AccuPyc II 1345 Densidad esquelética
ASTM D5604 Standard Test Methods for Precipitated Silica-Surface Area by Single Point B.E.T. Nitrogen Adsorption Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Single-point Specific Surface Area
ASTM D5861 Standard Guide for Significance of Particle Size Measurements of Coating Powders Saturn DigiSizer II 5205 Distribución del tamaño de las partículas
ASTM D5965 Standard Test Methods for Density of Coating Powders AccuPyc, AccuPyc II 1345 Densidad esquelética
ASTM D6093 Standard Test Method for Percent Volume Nonvolatile Matter in Clear or Pigmented Coatings Using a Helium Gas Pycnometer AccuPyc, AccuPyc II 1345 Densidad esquelética
ASTM D6226 Standard Test Method for Open Cell Content of Rigid Cellular Plastics AccuPyc, AccuPyc II 1345 Contenido de células abiertas y cerradas de la espuma
ASTM D6556 Standard Test Method for Carbon Black-Total and External Surface Area by Nitrogen Adsorption Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM D6761 Standard Test Method for Determination of the Total Pore Volume of Catalysts and Catalyst Carriers AutoPore V, AccuPyc, AccuPyc II 1345 Volumen total de poros
ASTM D7891-15 Standard Test Method for Shear Testing of Powders Using the Freeman Technology FT4 Reómetro de polvo FT4 Caracterización del cizallamiento del polvo
ASTM D8097 Standard Test Method for Determination of Bulk Density for Specific Size Fractions of Calcined Petroleum Coke Using a Transaxial Pressure Pycnometer GeoPyc Presión axial transversal (P.A.T.) Densidad
ASTM D8325 Standard Guide for Evaluation of Nuclear Graphite Surface Area and Porosity by Gas Adsorption Measurements Gemini, ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM E2864 Standard Test Method for Measurement of Airborne Metal Oxide Nanoparticle Surface Area Concentration in Inhalation Exposure Chambers using Krypton Gas Adsorption ASAP 2460 & 2425, TriStar II Plus, 3Flex Superficie específica
ASTM E2980 Standard Test Methods for Estimating Average Particle Size of Powders Using Air Permeability SAS Mean Particle Size & Envelope Specific Surface Area
ASTM F2149 Standard Test Method for Automated Analyses of Cells-the Electrical Sensing Zone Method of Enumerating and Sizing Single Cell Suspensions Elzone II 5390 Distribución del tamaño de las partículas
WK61828 Carbon Monoxide on Supported Platinum on Alumina Catalysts using Manometric Method ASAP 2020 Plus, 3Flex, ChemiSorb HTP Chemisorption; Catalyst Surface Area and Percent Dispersion
WK17123 New Test Method for Test Method for Carbon Monoxide Chemisorption on Supported Platinum on Alumina Catalysts using Dynamic Flow Method AutoChem III Chemisorption; Catalyst Surface Area and Percent Dispersion
WK71859 Carbon Monoxide Chemisorption on Supported Platinum on Alumina Catalysts using Static Vacuum Method ASAP 2020 Plus, 3Flex, ChemiSorb HTP Chemisorption; Catalyst Surface Area and Percent Dispersion
WK71860 Acid Site Characterization on Zeolites Using Dynamic Flow Method AutoChem III Caracterización de zonas ácidas
WK69721 Measuring the Permeability of Powders as a Function of Consolidation Using the Freeman Technology FT4 Reómetro de polvo FT4 Permeabilidad del polvo
WK69886 The Dynamic Testing of Powders using the Freeman Technology FT4 Reómetro de polvo FT4 Reología del polvo
USP Porosimetry by Mercury Intrusion USP Porosimetry by Mercury Intrusion AutoPore V Porosimetría de intrusión de mercurio
USP Laser Diffraction Measurement of Particle Size USP Laser Diffraction Measurement of Particle Size Saturn DigiSizer II 5205 Distribución del tamaño de las partículas
USP Gas Pycnometric Density of Solids USP Gas Pycnometric Density of Solids AccuPyc, AccuPyc II 1345 Densidad esquelética
USP Specific Surface Area USP Specific Surface Area Gemini, ASAP 2460 & 2425, TriStar II Plus Superficie específica

Malvern Panalytical Products by Industry Standards

Estándar Relevant Product(s) Notas
21 CFR Part 11 Aeris, MicroCal DSC, Empyrean, Epsilon, Mastersizer, Morphologi, OMNISEC, Spraytec, X’Pert 3, Zetasizer, Zetium View more information
ASTM D2622 Zetium Petro Factory guaranteed compliance to ASTM test methods
ASTM D4294 Epsilon 1 Sulphur in fuels Factory guaranteed compliance to ASTM test methods
ASTM D4326 Zetium Petro, Epsilon 4, Claisse LeNeo, Claisse Eagon 2, Claisse TheOx Advanced
ASTM D4927 Zetium Petro
ASTM D5059 Zetium Petro
ASTM D6334 Zetium Petro
ASTM D6376 Zetium Petro
ASTM D6443 Zetium Petro Factory guaranteed compliance to ASTM test methods
ASTM D6481 Epsilon 1 Lubricating oils
ASTM D7085 Zetium, Epsilon 1, Epsilon 4, Claisse LeNeo, Claisse Eagon 2, Claisse TheOx Advanced
ASTM D7751 Epsilon 4
ASTM C114 Zetium Petro
ICH Q3D Epsilon 4
IP 228 Epsilon 1 Sulphur in fuels, Zetium Petro Factory guaranteed compliance to IP test methods
IP 336 Epsilon 1 Sulphur in fuels, Epsilon 4 Factory guaranteed compliance to IP test methods
IP 352 Zetium Petro
IP 407 Zetium Petro
IP 433 Zetium Petro
IP 447 Zetium Petro
IP 489 Zetium Petro
IP 496 Epsilon 1 Sulphur in fuels, Epsilon 4 Factory guaranteed compliance to IP test methods
IP 497 Zetium Petro
IP 503 Zetium Petro
IP 593 Zetium Petro
ISO 13032 Epsilon 4, Epsilon 1 ISO 13032
ISO 14596 Zetium Petro
ISO 14597 Zetium Petro
ISO 15597 Zetium Petro
ISO 16258-1 View on MP page See source page
ISO 17025 XRF analysis services
ISO 17034 WROXI - Certified Reference Materials
ISO 19430 NanoSight
ISO 20847 Epsilon 1 Sulphur in fuels Factory guaranteed compliance to ISO test methods
ISO 20884 Zetium Petro
ISO 8754 Epsilon 1 Sulphur in fuels Factory guaranteed compliance to ISO test methods
ISO 29581-2 Zetium Cement, Epsilon 4
USP 232 Epsilon 4
USP 233 Epsilon 4