Capacity | Six ports |
Degas Method | Heat and vacuum |
Vacuum Control | Servo-controlled rates to minimize or eliminate sample elutriation |
Evacuation Rate | Selectable evacuation rate from 1.0 to 50.0 mmHg/s |
Heating of Samples | Heating mantles |
Temperature Range | 40 to 450 ºC in one degree increments |
Temperature Control | One ramp during evacuation phase, five additional ramps during subsequent phases |
Temperature Accuracy | Deviation less than ±10 ºC at the sensing thermocouple embedded in the heating mantle |
Heating Ramp Rate | Selectable from 0.1 ºC per minute to 10 ºC per minute |
Hold Time | Zero to 999 minutes in one-minute increments |
Backfill Options | Automatic backfill |
Dimensions | Height 69 cm (27 in.), Width 53 cm (21 in.), Depth 43 cm (17 in.) |
Weight | 70 lbs (32 kg) |
The Smart VacPrep is an advanced six-port system that utilizes vacuum to prepare samples by heating and evacuation. Each of the ports may be operated independently. Samples may be added or removed from degas ports without disturbing the treatment of other samples undergoing preparation. Degassing automatically terminates when the samples have completed all programmed steps.