Smart VacPrep

Smart VacPrep is an advanced six-port system that utilizes vacuum to prepare samples by heating and evacuation.

Specification

Capacidad

Six ports

Degas Method

Heat and vacuum

Vacuum Control

Servo-controlled rates to minimize or eliminate sample elutriation

Evacuation Rate

Selectable evacuation rate from 1.0 to 50.0 mmHg/s

Heating of Samples

Heating mantles

Temperatura

40 to 450 ºC in one degree increments

Temperature Control

One ramp during evacuation phase, five additional ramps during subsequent phases

Temperature Accuracy

Deviation less than ±10 ºC at the sensing thermocouple embedded in the heating mantle

Heating Ramp Rate

Selectable from 0.1 ºC per minute to 10 ºC per minute

Hold Time

Zero to 999 minutes in one-minute increments

Backfill Options

Automatic backfill

Dimensions

Height 69 cm (27 in.), Width 53 cm (21 in.), Depth 43 cm (17 in.)

Peso

70 lbs (32 kg)

Visión general

The Smart VacPrep is an advanced six-port system that utilizes vacuum to prepare samples by heating and evacuation. Each of the ports may be operated independently. Samples may be added or removed from degas ports without disturbing the treatment of other samples undergoing preparation. Degassing automatically terminates when the samples have completed all programmed steps.

Solicitar información

Smart VacPrep 067

Solicite un presupuesto o hable con un experto para obtener más información