Higher Accuracy Plus Faster Results When Measuringthe Density of Commercial Items

Density measurements have proven their value in a number of industries on a wide variety of materials. The AccuPyc 1330 can analyze organic or inorganic samples with a vapor pressure of less than 25 mmHg. Using helium gas, volumes of these materials can be measured to a precision of ± 0.02% with relative ease.

As a demonstration, the AccuPyc 1330 was used to measure the density of a wide variety of materials. The temperature of measurement was 28 °C ± 0.5 °C. Results of these measurements are shown below.

Measured Densities of Some Commercial Items

MaterialDensity (Standard Deviation)(g/cm3)
Lipstick0.9895± 0.0002
Toothpaste1.5178± 0.0002
Chocolate Candy
Milk
Nut
Dark
Crisped Rice

1.2908
1.1988
1.3083
1.1840

± 0.0003
± 0.0002
± 0.0005
± 0.0002
Petroleum Jelly0.8767± 0.0000
Peanut Butter
Creamy
Crunchy

1.1176
1.1046

± 0.0000
± 0.0001
Bath Soap
Floating
Other

0.9348
1.0400

± 0.0001
± 0.0001
Peanuts
Salted
Unsalted

1.0872
1.0934

± 0.0001
± 0.0003
Oil
Vacuum Pump
Motor
Diffusion Pump

0.8634
0.8837
1.0593

± 0.0000
± 0.0000
± 0.0001
Mercury, 28 °C13.5268± 0.0012
Putty
Play-Doh
Glazing compound
1.2979
2.1303
± 0.0002
± 0.0003
Paint
Rust preventative
Latex, white, indoor
Oil-based, outdoor
0.9666
1.2362
1.0034
± 0.0000
± 0.0002
± 0.0001
Mayonnaise
Hellmans
Miracle Whip
1.0228
1.0628
± 0.0002
± 0.0002
Mustard
English
Dijon

1.2213
1.0934

± 0.0003
± 0.0002

Conclusions
The AccuPyc 1330 is capable of rapid measurements of organic or inorganic densities to a precision of 0.02%. This precision is sufficient to detect variability of organic and inorganic materials with a given lot and to estimate the purity of the samples.